Cracks in buildings not only affect aesthetics but also compromise structural integrity and the durability of the coating. This article outlines how to treat different types of cracks to ensure long-lasting coating results.
I. Base Layer Crack Repair Solutions
Cracks are categorized into fine cracks (less than 0.5mm) and significant cracks (greater than 0.5mm).
1. Fine Cracks (Less than 0.5mm)
: Use a wire brush to remove dust; improper cleaning affects repair adhesion.
: Apply elastic anti-crack leveling putty to fill and smooth the cracks, ensuring no air gaps.
2. Significant Cracks (Greater than 0.5mm)
: Cut a U-shaped groove, clean the cracks, and repair with anti-crack putty.
: Inject low-viscosity epoxy resin, and apply reinforcement mesh to ensure structural stability.
II. Corner Treatment
1. Exterior Corner Treatment
: Use a level to protect the corner during application.
: Wait for each side to dry before spraying the other, preventing cross-contamination.
2. Interior Corner Treatment
: Use a chalk line for precise application.
: Same as exterior, ensure the surface is dry before applying the next coat.
III. Window and Door Corner Treatment
For window and door corners, ensure repair materials are fully cured before coating. Use reinforcement mesh with fast-drying materials to prevent future cracks.